Gilsonite in Foundry Sand: How It Works
Green sand moulding is the most common way to make iron castings. Carbonaceous additives are added to the…
Practical, expert articles on gilsonite in drilling fluids, asphalt, foundry, inks, paints, coatings and waterproofing.

Green sand moulding is the most common way to make iron castings. Carbonaceous additives are added to the…

Do I need special paving equipment? No. Normal pavers and rollers are used. Does gilsonite asphalt look different?…

When a road reaches the end of its surface life, an overlay restores ride quality and structure. Gilsonite…

Desert roads face extreme heat, wind-blown sand and large daily temperature swings. Granular gilsonite is easy to handle…

A gilsonite-modified pavement is only as good as the quality control behind it. Keep batch numbers of gilsonite…

Beyond normal roads, gilsonite-modified asphalt is used in several specialty pavements. Thin, stiff, waterproof surfacing layers protect the…

Freight corridors, quarry roads and port access roads carry far more trucks than ordinary roads. Their pavements need…

Pavement preservation means treating roads while they are still in good condition to extend their life at low…

Parking lots and driveways suffer from oil drips, sun exposure and turning tires. Gilsonite helps in both the…

Chip seals (surface dressing) are a low-cost way to waterproof and restore skid resistance to roads. The binder…

Warm mix asphalt (WMA) is produced at temperatures 20–40°C lower than hot mix, saving fuel and reducing emissions.…

Porous asphalt and open-graded friction courses (OGFC) drain water quickly, reduce spray and lower noise. But their open…
| Product | Particle size | Softening point (R&B) | Typical dosage | |
|---|---|---|---|---|
| Gilsonite Lump | 0 – 50 mm (custom) | 150 – 220 °C | Depends on application. | Spec · MSDS · COA |
| Gilsonite Granular | 1 – 5 mm | 150 – 200 °C | Asphalt: 4–12 % by weight of binder. | Spec · MSDS · COA |
| Gilsonite Powder | 100 – 200 mesh | 150 – 220 °C | Drilling 2–8 lb/bbl · asphalt 4–12 % of binder · foundry 0.3–1.0 % | Spec · MSDS · COA |
| Micronized Gilsonite | 300 – 600 mesh | 150 – 180 °C | Ink varnish: 20–40 % in oil. | Spec · MSDS · COA |
| Drilling Fluid Grade Gilsonite | 75 – 200 µm | 160 – 220 °C (grades) | 2 – 8 lb/bbl | Spec · MSDS · COA |
| Sulphonated Asphalt | — | — | 2 – 6 lb/bbl | Spec · MSDS · COA |
| Cementing Grade Gilsonite | 75 – 200 µm | 160 – 220 °C | 5 – 15 % BWOC | Spec · MSDS · COA |
| Asphalt Modifier Grade Gilsonite | Powder ≤ 200 mesh / granular 1–5 mm | 150 – 200 °C | 4 – 12 % by weight of binder | Spec · MSDS · COA |
| Foundry Grade Gilsonite | 100 – 300 mesh | 150 – 200 °C | 0.3 – 1.0 % (iron) | Spec · MSDS · COA |
| Ink & Paint Grade Gilsonite | 200 – 600 mesh | 150 – 180 °C | Ink varnish: 20–40 % in oil | Spec · MSDS · COA |
| Coating & Waterproofing Grade Gilsonite | ≤ 200 mesh | 150 – 200 °C | 5 – 25 % of compound | Spec · MSDS · COA |
| Sealer & Filler Grade Gilsonite | ≤ 200 mesh | 150 – 180 °C | Sealer: 15 – 35 % | Spec · MSDS · COA |
Get a quotation, samples and full documentation (TDS, MSDS, COA) within 24 hours.